Alloying: Understanding the Basics
Edited by
ASM International
ISBN electronic:
978-1-62708-297-6
Publication date:
2001
Search within book:
Abstract
This article discusses the compositions, properties, and uses of silver, gold, and platinum group metals, including platinum, rhodium, iridium, ruthenium, and osmium. It describes the role of various alloying elements and explains how they affect physical, mechanical, and electrical properties as well as corrosion resistance.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Noble Metal Alloys, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001, p 550–569, https://doi.org/10.31399/asm.tb.aub.t61170550
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Au (Gold) Ternary Alloy Phase Diagrams
Alloy Phase Diagrams
Annealing of Precious Metals
Heat Treating of Nonferrous Alloys
Resistance Brazing
Welding, Brazing, and Soldering
Filler Metals for Carat Gold and Hallmark Silver Jewelry
Principles of Brazing
Compacted Graphite Irons
Alloying Understanding the Basics
Austenitic Manganese Steels
Alloying Understanding the Basics
Vapor Phase Corrosion Inhibitors
Corrosion: Fundamentals, Testing, and Protection
Malleable Irons
Alloying Understanding the Basics
High-Alloy White Irons
Alloying Understanding the Basics
High-Strength Low-Alloy Steels
Alloying Understanding the Basics