Abstract
This article examines the composition and properties of magnesium and its alloys. It discusses alloy and temper designations, applications and product forms, and commercial alloy systems, and explains how alloying elements affect physical and mechanical properties, processing characteristics, and corrosion behaviors.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Magnesium and Magnesium Alloys, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001, p 432–453, https://doi.org/10.31399/asm.tb.aub.t61170432
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Ductile Irons
Alloying Understanding the Basics
Aluminum and Aluminum Alloys
Alloying Understanding the Basics
Malleable Irons
Alloying Understanding the Basics
Alloying of Beryllium
Beryllium Chemistry and Processing
Stainless Steels
Alloying Understanding the Basics
Nickel and Nickel Alloys
Alloying Understanding the Basics
Aluminum Alloys
Lightweight Materials Understanding the Basics
Carbon and Alloy Steels
Alloying Understanding the Basics
Metallography and Microstructures of Magnesium and Its Alloys
Metallography and Microstructures
Mechanical Behavior of High-Entropy Alloys—Questions and Answers
Mechanical Behavior of High-Entropy Alloys: Key Topics in Materials Science and Engineering