Ordered Intermetallics
-
Published:2001
Abstract
This article discusses the effect of alloying on the composition, structure, properties, and processing characteristics of ordered intermetallic compounds, including nickel aluminides, iron aluminides, and titanium aluminides. It includes several data tables along with a list of typical applications.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Ordered Intermetallics, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001, p 337–348, https://doi.org/10.31399/asm.tb.aub.t61170337
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Advanced Alloys and Future Directions
Titanium: A Technical Guide (Second Edition)
Compacted Graphite Irons
Alloying Understanding the Basics
Austenitic Manganese Steels
Alloying Understanding the Basics
Malleable Irons
Alloying Understanding the Basics
High-Alloy White Irons
Alloying Understanding the Basics
High-Strength Low-Alloy Steels
Alloying Understanding the Basics
Maraging Steels
Alloying Understanding the Basics
Titanium and Titanium Alloys
Alloying Understanding the Basics
Zinc and Zinc Alloys
Alloying Understanding the Basics
Cemented Carbides and Cermets
Alloying Understanding the Basics