This article discusses the effects of alloying on the properties and behaviors of maraging steels. It describes how maraging steels differ from conventional steels in that they are strengthened, not by carbon, but by the precipitation of intermetallic compounds. It explains how maraging steels typically have high levels of nickel, cobalt, and molybdenum with little carbon content and how that affects their dimensional stability, fracture toughness, weldability, and resistance to stress-corrosion cracking.
Maraging Steels, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001, p 234–241, https://doi.org/10.31399/asm.tb.aub.t61170234