Chapter 12: Corrosion
-
Published:2013
Abstract
This chapter discusses the formation and control of aqueous corrosion in iron and steel. It also provides information on passivation, stress corrosion, rust, and direct oxidation.
Topics
Aqueous corrosion
You do not currently have access to this chapter.
Citation
Corrosion, Elementary Materials Science, By William R. Hosford, ASM International, 2013, p 129–138, https://doi.org/10.31399/asm.tb.ems.t53730129
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Introduction and Overview of Electrochemical Corrosion
Fundamentals of Electrochemical Corrosion
Designing to Minimize Corrosion
Corrosion: Fundamentals, Testing, and Protection
Corrosion of Electronic Equipment in Military Environments
Corrosion: Environments and Industries
Military Specifications and Standards
Corrosion: Environments and Industries
Principles of Corrosion
Surface Engineering for Corrosion and Wear Resistance
Designing to Minimize Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Introduction to the Fundamentals of Corrosion
Corrosion: Fundamentals, Testing, and Protection
Effects of Metallurgical Variables on Aqueous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Corrosion in Service Water Distribution Systems
Corrosion: Environments and Industries
Corrosion in the Military
Corrosion: Environments and Industries