Chapter 6: Nonferrous Metals
-
Published:2013
Abstract
This chapter describes the properties and uses of aluminum, magnesium, titanium, and other nonferrous alloys. It also discusses the effect of cold working and the process of annealing, including recovery, recrystallization, and grain growth.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Nonferrous Metals, Elementary Materials Science, By William R. Hosford, ASM International, 2013, p 59–67, https://doi.org/10.31399/asm.tb.ems.t53730059
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Recovery, Recrystallization, and Grain-Growth Structures
Metallography and Microstructures
Mechanical Work of Steels—Cold Working
Metallography of Steels Interpretation of Structure and the Effects of Processing
Heat Treating of Brasses
Heat Treating of Nonferrous Alloys
Principles of Heat Treating of Nonferrous Alloys
Heat Treating of Nonferrous Alloys
Recovery, Recrystallization, and Grain Growth
Elements of Metallurgy and Engineering Alloys
Microstructure Modeling in Superalloy Forging
Cold and Hot Forging Fundamentals and Applications
Monte Carlo Models for Grain Growth and Recrystallization
Fundamentals of Modeling for Metals Processing
Heat Treating of Nonferrous Alloys
Practical Heat Treating (Second Edition)
Annealing and Recrystallization of Coppers
Heat Treating of Nonferrous Alloys
Work Hardening and Annealing of Aluminum Alloys
Aluminum Science and Technology