Chapter 4: Electrical Behavior
-
Published:2013
Abstract
This chapter examines some of the behaviors that suit materials for electrical and electronic applications. It begins by explaining how charge carriers move in metals and semiconductors and how properties such as conductivity, mobility, and resistivity are derived. It discusses the significance of energy bands, intrinsic and extrinsic conduction, and the properties of compound semiconductors. It also covers semiconductor devices, including p-n junctions, light emitting diodes, transistors, and piezoelectric crystals.
You do not currently have access to this chapter.
Citation
Electrical Behavior, Elementary Materials Science, By William R. Hosford, ASM International, 2013, p 37–49, https://doi.org/10.31399/asm.tb.ems.t53730037
Download citation file:
Related Book Content
Failure Analysis and Reliability of Optoelectronic Devices
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Transistor Characterization: Physics and Instrumentation
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Silicon Device Backside De-Processing and Fault Isolation Techniques
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
The Fundamentals of Nanoprobe Analysis
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)