Chapter 6: Engineering Die Castings
-
Published:2018
Abstract
The die casting process is a widely applied technique used by a variety of industries. This chapter reviews the casting design and engineering requirements for optimizing the characteristics of die castings.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Engineering Die Castings, Aluminum Castings Engineering Guide, By Jagan Nath, ASM International, 2018, p 103–149, https://doi.org/10.31399/asm.tb.aceg.t68410103
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Sand Casting of Aluminum Alloys
Aluminum Science and Technology
Intergranular Corrosion Failure in Zn-Al Alloy Solenoid Valve Seats
Handbook of Case Histories in Failure Analysis
Metal Waves or Laking on Zinc-Based Diecastings
ASM Failure Analysis Case Histories: Processing Errors and Defects
Broken Full Lift Disk of a Safety Valve
ASM Failure Analysis Case Histories: Mechanical and Machine Components
Casting Design and Quality Assurance
Metals Handbook Desk Edition (2nd Edition)
Pattern Equipment
Steel Castings Handbook (Sixth Edition)
Casting Design and Processes
Casting
Fatigue and Fracture Properties of Aluminum Alloy Castings
Fatigue and Fracture
Plating Blemishes in Zinc Die Castings
ASM Failure Analysis Case Histories: Processing Errors and Defects
380.0, A380.0, and B380.0 General-Purpose Die-Casting Alloys
Properties and Selection of Aluminum Alloys