Chapter 4: Overview of Casting Processes
-
Published:2018
Abstract
This chapter discusses the advantages, limitations, and applications of various aluminum casting processes, namely green sand casting process, air set or no-bake molding process, vacuum molding process, evaporative foam casting process, and die casting process. The processes covered also include gravity permanent molding, low-pressure permanent molding, counter pressure, squeeze casting, investment casting, rapid prototype casting, cast forge hybrid, and semisolid metal processes.
Sign in
ASM members
Member Sign InOverview of Casting Processes, Aluminum Castings Engineering Guide, By Jagan Nath, ASM International, 2018, p 29–90, https://doi.org/10.31399/asm.tb.aceg.t68410029