Chapter 7: Testing and Inspection of Metals—The Quest for Quality
-
Published:2011
Abstract
This chapter explains how metallography and hardness testing are used to evaluate the quality and condition of metal products. It also discusses the use of tensile testing, fracture toughness and impact testing, fatigue testing, and nondestructive test methods including ultrasonic, x-ray, and eddy current testing.
You do not currently have access to this chapter.
Citation
Testing and Inspection of Metals—The Quest for Quality, Metallurgy for the Non-Metallurgist, 2nd ed., Edited By Arthur C. Reardon, ASM International, 2011, p 149–174, https://doi.org/10.31399/asm.tb.mnm2.t53060149
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Inspection Methods: Overview and Comparison
Inspection of Metals Understanding the Basics
Standards and Inspection
Practical Induction Heat Treating (Second Edition)
Overview of Mechanical Properties and Testing for Design
Mechanical Testing and Evaluation
Mechanical Testing
Metals Handbook Desk Edition (2nd Edition)
Glossary of Terms
Tensile Testing (Second Edition)
Tensile Testing of Elastomers
Tensile Testing (Second Edition)
The Fundamentals of Hardness Testing
Hardness Testing Principles and Applications
Hardness
Metallography Principles and Practice
Standards and Codes for Nondestructive Testing
Nondestructive Evaluation of Materials
Tensile Testing of Plastics
Tensile Testing (Second Edition)