Corrosion in the Petrochemical Industry (Second Edition)
Abstract
This chapter focuses on stress-corrosion cracking (SCC) of metals and their alloys. It is intended to familiarize the reader with the phenomenological and mechanistic aspects of stress corrosion. The phenomenological description of crack initiation and propagation describes well-established experimental evidence and observations of stress corrosion, while the discussions on mechanisms describe the physical process involved in crack initiation and propagation. Several parameters that are known to influence the rate of crack growth in aqueous solutions are presented, along with important fracture features.
Sign in
ASM members
Member Sign InStress-Corrosion Cracking, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 126–147, https://doi.org/10.31399/asm.tb.cpi2.t55030126
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.