This chapter discusses five forms of mechanically assisted degradation of metals: erosion, fretting, fretting fatigue, cavitation and water drop impingement, and corrosion fatigue. Emphasis is placed on the mechanisms and the factors affecting these forms of degradation.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Forms of Mechanically Assisted Degradation, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 117–125, https://doi.org/10.31399/asm.tb.cpi2.t55030117
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Forms of Mechanically Assisted Degradation
Corrosion: Fundamentals, Testing, and Protection
Evaluating Erosion Corrosion, Cavitation, and Impingement
Corrosion: Fundamentals, Testing, and Protection
Types of Wear and Erosion and Their Mechanisms
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Military Aircraft Corrosion Fatigue
Corrosion: Environments and Industries
Fretting Fatigue
Fatigue and Fracture
Corrosion
Elements of Metallurgy and Engineering Alloys
Failure of a Fuel Pump in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Erosion and Erosion-Corrosion
High-Temperature Corrosion and Materials Applications
Failure of a Fan Support Casting
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Erosion, Cavitation, Impingement, and Fretting Corrosion
Corrosion of Aluminum and Aluminum Alloys