Abstract
This chapter discusses various factors that affect corrosion of stainless steel weldments. It begins by providing an overview of the metallurgical factors associated with welding. This is followed by a discussion on preferential attack associated with weld metal precipitates in austenitic stainless steels as well as several forms of corrosion associated with welding. The effects of gas-tungsten arc weld shielding gas composition and heat-tint oxides on corrosion resistance are then covered. Microbiological corrosion of butt welds in water tanks is also illustrated. In addition, the chapter provides information on corrosion of ferritic and duplex stainless steel weldments.
Corrosion of Stainless Steel Weldments, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 96–111, https://doi.org/10.31399/asm.tb.cpi2.t55030096