Abstract
This chapter describes the effects of metallurgical variables on the corrosion of aluminum alloys. Emphasis is placed on the effect of constituent particles on pitting corrosion of aluminum.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 70–73, https://doi.org/10.31399/asm.tb.cpi2.t55030070
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion: Fundamentals, Testing, and Protection
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology
Aluminum—The Light Metal
The History of Metals in America
Understanding the Corrosion Behavior of Aluminum
Corrosion of Aluminum and Aluminum Alloys
Types of Corrosive Environments
Corrosion of Aluminum and Aluminum Alloys
Etching of Aluminum and Its Alloys
Aluminum Science and Technology
Introduction
Corrosion of Aluminum and Aluminum Alloys
Temper Designations for Aluminum and Aluminum Alloys
Corrosion of Aluminum and Aluminum Alloys