This chapter is a detailed account of major sources of stray current that can cause corrosion and discusses several ways to prevent damage from stray-current corrosion.
Topics
Stray current corrosion
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Stray-Current Corrosion, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 23–24, https://doi.org/10.31399/asm.tb.cpi2.t55030023
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Galvanic, Deposition, and Stray-Current Corrosion
Corrosion of Aluminum and Aluminum Alloys
External Corrosion of Oil and Natural Gas Pipelines
Corrosion in the Petrochemical Industry (Second Edition)
Coping with Corrosion
Metallurgy for the Non-Metallurgist (Second Edition)
Uniform Corrosion of a Copper Pipe Coupling
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure
Military Specifications and Standards
Corrosion: Environments and Industries
Microbiologically Influenced Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion-Fatigue Cracking of Gray Iron Cylinder Inserts From a Water-Cooled Locomotive Diesel Engine
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Corrosion in the Military
Corrosion: Environments and Industries
Analysis and Prevention of Environmental- and Corrosion-Related Failures
Failure Analysis and Prevention (2021 Edition)
Petroleum Industry Applications
Stainless Steels for Design Engineers