This article depicts typical fractographic features for a number of different composite materials, covering interlaminar and translaminar fracture characteristics in composite materials.
You do not currently have access to this chapter.
Citation
Fractography of Composites, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 417–429, https://doi.org/10.31399/asm.tb.cfap.t69780417
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Fractography
Composites
Fatigue Fracture Appearances
Failure Analysis and Prevention
Publication History
Fractography
Credits
Fractography
Repair
Structural Composite Materials
Glossary of Filament-Winding Terms
Composite Filament Winding
Failure of a Throttle End Fitting in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Out-of-Plane Analysis
Composites
Porous Powder Metallurgy Technology
Powder Metallurgy