Characterization and Failure Analysis of Plastics
Abstract
This article reviews various analytical techniques most commonly used in plastic component failure analysis. The description of the techniques is intended to make the reader familiar with the general principles and benefits of the methodologies. The descriptions of the analytical techniques are supplemented by a series of case studies that include pertinent visual examination results and the corresponding images that aided in the characterization of the failures. The techniques covered include Fourier transform infrared spectroscopy, differential scanning calorimetry, thermogravimetric analysis, thermomechanical analysis, and dynamic mechanical analysis. The article also discusses various analytical methods used to characterize the molecular weight...
Sign in
ASM members
Member Sign InCharacterization of Plastics in Failure Analysis, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 359–382, https://doi.org/10.31399/asm.tb.cfap.t69780359
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.