Characterization and Failure Analysis of Plastics
Abstract
This article introduces procedures an engineer or materials scientist can use to investigate failures. It provides a brief survey of polymer systems and key properties that need to be measured during failure analysis. The article begins with an overview of the problem-solving approach pertinent to structure analysis. This is followed by a review of the characterization of plastics by infrared and nuclear magnetic resonance spectroscopy. The article then provides information on the distribution of molecular weight of an engineering plastic. It further discusses the methods used in thermal analysis, namely differential thermal analysis, thermogravimetric analysis, thermal-mechanical analysis, and dynamic...
Sign in
ASM members
Member Sign InAnalysis of Structure, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 343–358, https://doi.org/10.31399/asm.tb.cfap.t69780343
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.