Characterization and Failure Analysis of Plastics
Edited by
ASM International
ISBN electronic:
978-1-62708-281-5
Publication date:
2003
Abstract
This article is a detailed account of the mechanisms of fatigue failure of polymers, namely thermal fatigue failure and mechanical fatigue failure. The mechanical fatigue failure is discussed in terms of fatigue crack initiation and fatigue crack propagation.
You do not currently have access to this chapter.
Citation
Fatigue Failure Mechanisms, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 249–258, https://doi.org/10.31399/asm.tb.cfap.t69780249
Download citation file:
Related Book Content
Fatigue Testing and Behavior of Plastics
Mechanical Testing and Evaluation
Nonarbitrary Crack Size Concept for Fatigue Crack Initiation
Mechanics and Mechanisms of Fracture An Introduction
P/M Aluminum Alloys: Atlas of Fractographs
Fractography
Polymers: Atlas of Fractographs
Fractography
Fatigue
Elements of Metallurgy and Engineering Alloys
Dies and Die Materials for Hot Forging
Metalworking: Bulk Forming
Fatigue of Metals
Fatigue and Fracture Understanding the Basics
Fundamentals of Modern Fatigue Analysis for Design
Fatigue and Fracture
Failure of a Gear in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Elevated-Temperature Failures
Understanding How Components Fail (Third Edition)