Characterization and Failure Analysis of Plastics
Edited by
ASM International
ISBN electronic:
978-1-62708-281-5
Publication date:
2003
Abstract
This article reviews fatigue test methodologies, provides an overview of general fatigue behavior (crack initiation and propagation) in engineering plastics, and discusses some of the factors affecting the fatigue performance of polymers. In addition, it provides information on fractography that provides useful insight into the nature of fracture processes.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Fatigue Testing and Behavior, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 238–248, https://doi.org/10.31399/asm.tb.cfap.t69780238
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Malleable Irons/White Irons: Atlas of Fractographs
Fractography
Mechanisms of Stress-Corrosion Cracking
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking
Corrosion in the Petrochemical Industry (Second Edition)
Stress-Corrosion Cracking
Corrosion: Fundamentals, Testing, and Protection
Failure of a First-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Fracture and Fractography
Characterization and Failure Analysis of Plastics
Fatigue Strength of Metals
Mechanics and Mechanisms of Fracture An Introduction
Cracking in an Aircraft Nose Landing Gear Strut
Handbook of Case Histories in Failure Analysis
Fracture Analysis
Cast Iron Science and Technology