Characterization and Failure Analysis of Plastics
Design and Selection of Plastics Processing Methods
-
Published:2003
Abstract
This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts and includes a discussion on materials and process selection methodology for plastics. The discussion covers the primary plastic processing methods and how each process influences part design and the properties of the plastic part. It also includes a brief description of functional requirements in process selection; an overview of various process effects and how they affect the functions and properties of the part; and the selection of processes for size, shape, and design detail factors.
Sign in
ASM members
Member Sign InDesign and Selection of Plastics Processing Methods, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 64–86, https://doi.org/10.31399/asm.tb.cfap.t69780064
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.