Effects of Composition, Processing, and Structure on Properties of Engineering Plastics[1]
-
Published:2003
Abstract
This article describes in more detail the fundamental building-block level, atomic, then expands to a discussion of molecular considerations, intermolecular structures, and finally supermolecular issues. An explanation of important thermal, mechanical, and physical properties of engineering plastics and commodity plastics follows, and the final section briefly outlines the most common plastics manufacturing processes.
Sign in
ASM members
Member Sign InEffects of Composition, Processing, and Structure on Properties of Engineering Plastics, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 28–48, https://doi.org/10.31399/asm.tb.cfap.t69780028
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.