Chapter 12: Consequences of Using Advanced High-Strength Steels
-
Published:2013
Abstract
This chapter describes the nature of the problems arising from using advanced high-strength steels (AHSS) and discusses potential remedies to minimize the adverse effects that may limit the adoption of AHSS in the automotive industry. The discussion provides information on press energy, springback, residual stress, die wear, hot forming, downgaging limits, welding, binders, draw beads, and tool material wear.
Consequences of Using Advanced High-Strength Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 177–198, https://doi.org/10.31399/asm.tb.ahsssta.t53700177