Book Chapter
Chapter 9: Twinning-Induced Plasticity Steels
-
Published:2013
Abstract
This chapter briefly discusses the characteristics of mechanical twins and stacking faults in close-packed planes. It provides an overview of the composition, microstructures, thermodynamics, processing, deformation mechanism, mechanical properties, formability, and special attributes of twinning-induced plasticity steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Twinning-Induced Plasticity Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 135–149, https://doi.org/10.31399/asm.tb.ahsssta.t53700135
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Steel Fundamentals
Advanced-High Strength Steels Science, Technology, and Applications
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications
Alteration of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Heat Treating of Magnesium Alloy Metal-Matrix Composites
Heat Treating of Nonferrous Alloys
Nanofluids as Quenchants in Industrial Heat Treatment
Steel Heat Treating Technologies
Heat Treatment of Copper Precipitation-Strengthened Steels
Heat Treating of Irons and Steels