Chapter 8: Martensitic Steels
-
Published:2013
Abstract
Martensitic steels are produced by quenching carbon steel from the austenite phase into martensite. This chapter provides information on the composition, microstructures, processing, deformation mechanisms, mechanical properties, hot forming, tempering, and special attributes of martensitic steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Martensitic Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 127–133, https://doi.org/10.31399/asm.tb.ahsssta.t53700127
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Tempering of Steel
Steels: Processing, Structure, and Performance (Second Edition)
Tempering of Induction Hardened Steels
Induction Heating and Heat Treatment
Introduction to the Mechanical Behavior of Metals
Mechanical Testing and Evaluation
Tempering
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels