Skip Nav Destination
View Technical Books >
ASM Technical Books
Advanced-High Strength Steels: Science, Technology, and Applications
ASM International
ISBN electronic:
978-1-62708-279-2
Publication date:
2013
Book Chapter
Chapter 5: Dual-Phase Steels
-
Published:2013
Search within book:
Abstract
Dual-phase (DP) steels have the widest usage in automotive industry because of their excellent combination of strength and ductility. This chapter provides an overview of the composition, microstructure, processing, deformation mechanism, mechanical properties, formability, and special attributes of DP steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Dual-Phase Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 95–106, https://doi.org/10.31399/asm.tb.ahsssta.t53700095
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Dual-Phase Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Steel Fundamentals
Advanced-High Strength Steels Science, Technology, and Applications
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications
Alteration of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Nanofluids as Quenchants in Industrial Heat Treatment
Steel Heat Treating Technologies
Heat Treating of Magnesium Alloy Metal-Matrix Composites
Heat Treating of Nonferrous Alloys