Chapter 4: Attributes of Advanced High-Strength Steels
-
Published:2013
Abstract
This chapter summarizes the performance attributes of advanced high-strength steels, namely stiffness, strength, strain hardening, fatigue, crashworthiness, formability, toughness, and bake hardening.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Attributes of Advanced High-Strength Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 71–94, https://doi.org/10.31399/asm.tb.ahsssta.t53700071
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Steel Products and Properties
Metallurgy for the Non-Metallurgist (Second Edition)
Design with Plastics
Materials Selection and Design
Design with Plastics
Characterization and Failure Analysis of Plastics
Mechanical Behavior
Elements of Metallurgy and Engineering Alloys
Influence of Work Material Properties on Finishing Methods
Surface Engineering
Introduction
Advanced-High Strength Steels Science, Technology, and Applications
Applications of Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
Global Projects on Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
Torch Soldering
Welding, Brazing, and Soldering
Evolving Advanced High-Strength Steel Grades
Advanced-High Strength Steels Science, Technology, and Applications