The History of Metals in America
Chapter Six: The Toolmakers
-
Published:2018
Abstract
This chapter provides a detailed account of the development of tool steel technology. It begins with a record of steelmaking in ancient and medieval times. The crucible melting process involved in making steel is then discussed. This is followed by a description of the increasing use of alloys for tool steels. The chapter provides information on the research investigations into the metallurgy of high-speed tool steels at MIT, Union Carbide, and Carbon Laboratories. The major research effort involved in substituting molybdenum for tungsten in high-speed tool steels is discussed. The chapter also describes the role of the Cleveland Twist...
Sign in
ASM members
Member Sign InThe Toolmakers, The History of Metals in America, By Charles R. Simcoe;Edited By Frances Richards, ASM International, 2018, p 73–91, https://doi.org/10.31399/asm.tb.hma.t59250073
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.