Abstract
This chapter discusses the evolution of engineering alloy steels, namely chromium, nickel, and nickel-chromium alloy steels. The discussion includes the automotive demand and development of specifications for the alloy steels. It also covers various research on heat treatment of alloy steels, providing information on hardening, transformation of austenite, hardenability testing, and tempering of as-quenched martensite.
You do not currently have access to this chapter.
Citation
The History of Engineering Alloy Steels, The History of Metals in America, By Charles R. Simcoe;Edited By Frances Richards, ASM International, 2018, p 59–72, https://doi.org/10.31399/asm.tb.hma.t59250059
Download citation file:
Related Book Content
Continuous Cooling Diagrams of Selected Steels
Failure Analysis of Heat Treated Steel Components
Heating and Holding Times
Steel Heat Treating Technologies
Iron and Steel
Elementary Materials Science
Temper Colors for Steels
Heat Treating of Irons and Steels
Water-Hardening Tool Steels
Tool Steels (Fifth Edition)
Air-Hardening, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Acoustical Characterization
Steel Heat Treating Technologies
High-Carbon, High-Chromium, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Oil-Hardening Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Mold Steels
Tool Steels (Fifth Edition)