Chapter 5: Investment Casting
-
Published:2002
Abstract
This chapter discusses the application of investment casting to nickel- and cobalt-base superalloys. It describes the production of polycrystalline and single crystal castings, the materials normally used, and the part dimensions and tolerances typically achieved. It explains how patterns, molds, and shells are produced, discusses the practice of directional solidification, and examines an assortment of turbine components cast from nickel- and cobalt-base alloys. The chapter also addresses casting problems such as inclusions, porosity, distortion, core shift, and leaching and explains how to avoid them.
Investment Casting, Superalloys: A Technical Guide, 2nd ed., By Matthew J. Donachie, Stephen J. Donachie, ASM International, 2002, p 79–90, https://doi.org/10.31399/asm.tb.stg2.t61280079