This chapter provides basic materials selection information for iron-nickel-, nickel-, and cobalt-base superalloys. It discusses mechanical and physical properties, the effect of service temperature, and the comparative strengths of wrought and cast product forms. It includes several large data tables along with reference information and a detailed application example based on the design of a gas turbine disk.
You do not currently have access to this chapter.
Citation
Selection of Superalloys, Superalloys: A Technical Guide, 2nd ed., By Matthew J. Donachie, Stephen J. Donachie, ASM International, 2002, p 11–24, https://doi.org/10.31399/asm.tb.stg2.t61280011
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Superalloys
Metals Handbook Desk Edition (2nd Edition)
333.0 and A333.0 Al-Si-Cu Permanent-Mold Casting Alloy
Properties and Selection of Aluminum Alloys
Properties of Metals
Metals Handbook Desk Edition (2nd Edition)
Structure/Property Relationships in Irons and Steels
Metals Handbook Desk Edition (2nd Edition)
Compositional Effects
Superalloys Alloying and Performance
Powder Metallurgy Superalloys
Powder Metallurgy
Structural Alloys
Materials at Low Temperatures
Other Sources
Superalloys: A Technical Guide (Second Edition)
Superalloys—Retrospect and Future Prospects
Superalloys: A Technical Guide (Second Edition)
Introduction
Superalloys Alloying and Performance