Appendix 1: Compositions
-
Published:2008
Abstract
This appendix contains tables listing the composition of austenitic, ferrite, martensitic, precipitation-hardenable, and duplex stainless steels and of Alloy Casting Institute heat- and corrosion-resisting casting alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Compositions, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 269–278, https://doi.org/10.31399/asm.tb.ssde.t52310269
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Wrought Stainless Steels: Selection and Application
Metals Handbook Desk Edition (2nd Edition)
Thermal Processing
Stainless Steels for Design Engineers
Stainless Steels
Alloying Understanding the Basics
Stainless Steels
Metallography of Steels Interpretation of Structure and the Effects of Processing
Stainless Steels
Metallurgy for the Non-Metallurgist (Second Edition)
Heat Treatment of Stainless Steels
Practical Heat Treating Basic Principles
Alloy Classification and Compositions
Powder Metallurgy
Introduction to the Selection of Stainless Steels
Welding, Brazing, and Soldering
Effects of Metallurgical Variables on the Corrosion of Stainless Steels
Corrosion: Fundamentals, Testing, and Protection
Heat Treating of Austenitic and Duplex Stainless Steels
Heat Treating of Irons and Steels