Abstract
This chapter discusses various factors pertinent to the prevention of corrosion in alloys for petroleum applications and reviews the selection of stainless steels for petroleum applications, including oil country tubular goods, line pipe, offshore platforms, liquefied natural gas vessels, and refinery equipment.
You do not currently have access to this chapter.
Citation
Petroleum Industry Applications, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 247–255, https://doi.org/10.31399/asm.tb.ssde.t52310247
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Corrosion Theory
Stainless Steels for Design Engineers
Stray-Current Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Failure Analysis of Cracks Formed at Extrados of Bend Pipe of API 5L X65M Grade
Handbook of Case Histories in Failure Analysis
Military Specifications and Standards
Corrosion: Environments and Industries
Microbiologically Influenced Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion-Fatigue Cracking of Gray Iron Cylinder Inserts From a Water-Cooled Locomotive Diesel Engine
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Corrosion in the Military
Corrosion: Environments and Industries
Galvanic, Deposition, and Stray-Current Corrosion
Corrosion of Aluminum and Aluminum Alloys
The Life of Harry Brearley (1871–1948)
The History of Stainless Steel
The Early Books and Papers on Stainless Steel (1917–1949)
The History of Stainless Steel