Skip Nav Destination
ASM Technical Books
Stainless Steels for Design Engineers
ASM International
ISBN electronic:
978-1-62708-286-0
Publication date:
2008
Book Chapter
Chapter 21: Marine Systems Applications
-
Published:2008
Abstract
This chapter reviews the major marine applications of stainless steels, including the desalination equipment, shipping containers, and heat exchangers that handle seawater.
You do not currently have access to this chapter.
Citation
Marine Systems Applications, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 243–246, https://doi.org/10.31399/asm.tb.ssde.t52310243
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Corrosion-Resistant Powder Metallurgy Alloys
Corrosion: Materials
Electrical Discharge Grinding
Machining
Introduction to Powder Metallurgy Stainless Steels
Powder Metallurgy
Failure of Large Tantalum Heat Exchanger During Transportation to Site
ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions
Failure Analysis of Heat Exchangers
Analysis and Prevention of Component and Equipment Failures
Sintering of Stainless Steels
Powder Metallurgy
Flux Cored Arc Welding
Welding Fundamentals and Processes
Corrosion Fatigue and Stress-Corrosion Cracking in Metallic Biomaterials
Corrosion: Environments and Industries
Tribological Properties of Stainless Steel and Other Corrosion-Resisting Metals
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications