Chapter 21: Marine Systems Applications
-
Published:2008
Abstract
This chapter reviews the major marine applications of stainless steels, including the desalination equipment, shipping containers, and heat exchangers that handle seawater.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Marine Systems Applications, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 243–246, https://doi.org/10.31399/asm.tb.ssde.t52310243
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Failure of Large Tantalum Heat Exchanger During Transportation to Site
ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions
Failure Analysis of Heat Exchangers
Analysis and Prevention of Component and Equipment Failures
Electrical Discharge Grinding
Machining
Corrosion-Resistant Powder Metallurgy Alloys
Corrosion: Materials
Introduction to Powder Metallurgy Stainless Steels
Powder Metallurgy
Case of Metal Dusting on HK40 HyL III Radiant Pipe Heat Exchanger
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Sintering of Stainless Steels
Powder Metallurgy
Types of Heat Treating Furnaces
Steel Heat Treating Technologies
Stress-Corrosion Cracking of Stainless Steel Falling Film Black Liquor Evaporator
ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment