Chapter 9: Transformation of Austenite
-
Published:1999
Abstract
This chapter discusses the isothermal transformation of austenite to pearlite, bainite, martensite, proeutectoid ferrite, and proeutectoid cementite. It describes the transformation mechanisms in eutectoid, hypoeutectoid, and hypereutectoid steels, the factors that influence nucleation and growth, and the characteristic features of the various microstructures. It also describes the transformation of austenite during continuous cooling.
You do not currently have access to this chapter.
Citation
Transformation of Austenite, Light Microscopy of Carbon Steels, By Leonard E. Samuels, ASM International, 1999, p 221–281, https://doi.org/10.31399/asm.tb.lmcs.t66560221
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Steels in the Annealed and Normalized Conditions
Light Microscopy of Carbon Steels
Microstructures, Processing, and Properties of Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Introduction to Steel Heat Treatment
Steel Heat Treating Fundamentals and Processes
Effects of Composition, Processing, and Structure on Properties of Irons and Steels
Materials Selection and Design
Fundamentals of Steel Heat Treatment
Practical Heat Treating Basic Principles
Conventional Heat Treatments—Usual Constituents and Their Formation
Metallography of Steels Interpretation of Structure and the Effects of Processing
Corrosion of Cast Irons
Corrosion: Materials
Properties of Iron
Heat Treatment of Gears A Practical Guide for Engineers
Bainitic Structures
Metallography and Microstructures
Bainite
Steels: Processing, Structure, and Performance (Second Edition)