Chapter 7: Metallographic Specimen Preparation
-
Published:2002
Abstract
This chapter instructs the metallographer on the basic skills required to prepare a polished metallographic specimen. It is organized in a chronological sequence starting with the information-gathering process on the material being investigated, then moving on to sectioning, mounting, grinding, and polishing processes, and ending with methods used to properly store metallographic specimens. The discussion covers the preparation procedures, the materials being investigated, and equipment used to perform these procedures.
Sign in
ASM members
Member Sign InMetallographic Specimen Preparation, Metallographer’s Guide: Practices and Procedures for Irons and Steels, By Bruce L. Bramfitt, Arlan O. Benscoter, ASM International, 2002, p 169–213, https://doi.org/10.31399/asm.tb.mgppis.t60400169
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.