Abstract
This chapter introduces the metallographer to the various types of steels and cast irons and explains how they are classified and defined. Classification and designation details are provided for plain carbon steels, alloy steels, and gray, white, ductile, and malleable cast irons.
You do not currently have access to this chapter.
Citation
Introduction to Steels and Cast Irons, Metallographer’s Guide: Practices and Procedures for Irons and Steels, By Bruce L. Bramfitt, Arlan O. Benscoter, ASM International, 2002, p 1–21, https://doi.org/10.31399/asm.tb.mgppis.t60400001
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Glossary
Metallographer’s Guide Practices and Procedures for Irons and Steels
Glossary of Terms: Surface Engineering
Surface Engineering
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Metallography and Microstructures of Cobalt and Cobalt Alloys
Metallography and Microstructures
Introduction—An Overview of Microstructure in Materials
Thermodynamics of Microstructures
Glossary of Terms: Composites
Composites
Tables Helpful to the Metallographer
Metallographer’s Guide Practices and Procedures for Irons and Steels
Fundamentals of the Heat Treating of Steel
Practical Heat Treating (Second Edition)
Microstructures of Nitrided Iron and Steel
Practical Nitriding and Ferritic Nitrocarburizing
Low-Alloy Special-Purpose Tool Steels
Tool Steels (Fifth Edition)