Steels: Processing, Structure, and Performance (Second Edition)
Chapter 21: Surface Hardening
-
Published:2015
Mechanical components often require surface treatments to meet application demands. This chapter describes several surface hardening treatments for steel and their effect on microstructure, composition, and properties. It discusses flame hardening, induction heating, carburizing, nitriding, carbonitriding, and nitrocarburizing. The discussion on carburizing addresses several interrelated factors, including processing principles, alloying, surface oxidation, residual stresses, bending fatigue, contact fatigue, and fracture.
Sign in
ASM members
Member Sign InSurface Hardening, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 499–549, https://doi.org/10.31399/asm.tb.spsp2.t54410499
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.