Steels: Processing, Structure, and Performance (Second Edition)
Chapter 20: Residual Stresses, Distortion, and Heat Treatment
-
Published:2015
Temperature and deformation gradients developed in the course of manufacturing can have undesired effects on the microstructures along their path; the two most common being residual stress and distortion. This chapter discusses these manufacturing-related problems and how they can be minimized by heat treatments. It also provides information on residual stress evaluation and prediction techniques.
Sign in
ASM members
Member Sign InResidual Stresses, Distortion, and Heat Treatment, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 487–497, https://doi.org/10.31399/asm.tb.spsp2.t54410487