Steels: Processing, Structure, and Performance (Second Edition)
Chapter 18: Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
-
Published:2015
Abstract
Steels with martensitic and tempered martensitic microstructures, though sometimes perceived as brittle, exhibit plasticity and ductile fracture behavior under certain conditions. This chapter describes the alloying and tempering conditions that produce a ductile form of martensite in low-carbon steels. It also discusses the effect of tempering temperature on the mechanical behavior and deformation properties of medium-carbon steels.
Sign in
ASM members
Member Sign InDeformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 405–437, https://doi.org/10.31399/asm.tb.spsp2.t54410405
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!