Chapter 17: Tempering of Steel
-
Published:2015
Most steels that are hardened are subjected to a subcritical heat treatment referred to as tempering. Tempering improves the toughness of as-quenched martensitic microstructures but lowers strength and hardness. This chapter describes the microstructural changes that occur during tempering and their effect on the mechanical properties of steel. It also discusses the effect of alloying elements and the formation of oxide colors.
You do not currently have access to this chapter.
Citation
Tempering of Steel, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 373–403, https://doi.org/10.31399/asm.tb.spsp2.t54410373
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)
Water-Hardening Tool Steels
Tool Steels (Fifth Edition)
Air-Hardening, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
High-Carbon, High-Chromium, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications
Tempering
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Oil-Hardening Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Heat Treating of Hot-Work Tool Steels
Heat Treating of Irons and Steels
Carburizing and Hardening Gears
Heat Treatment of Gears A Practical Guide for Engineers