This chapter discusses the stress-strain response of ferritic microstructures and its influence on tensile deformation, strain hardening, and ductile fracture of carbon steels. It describes the ductile-to-brittle transition that occurs in bcc ferrite, the effects of aging and grain size on strength and toughness, continuous and discontinuous yielding behaviors, and dispersion and solid-solution strengthening processes.
Topics
Microstructure,
Deformation and fracture,
Embrittlement,
High-carbon steel,
Low-carbon steel,
Medium-carbon steel,
Stainless steel,
Tool steel,
Surface hardening,
Tempering,
Steelmaking,
Surface treatment,
Hardenability,
Plastic deformation properties,
Aging,
Ductile-to-brittle transition temperature,
Stress-strain curves,
Ferrite
You do not currently have access to this chapter.
Citation
Deformation, Strengthening, and Fracture of Ferritic Microstructures, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 213–232, https://doi.org/10.31399/asm.tb.spsp2.t54410213
Download citation file:
Related Book Content
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)
Cyclic Stress-Strain Response and Microstructure
Fatigue and Fracture
Deformation and Recrystallization of Titanium and Its Alloys
Heat Treating of Nonferrous Alloys
Mechanisms and Causes of Failures in Heat Treated Steel Parts
Failure Analysis of Heat Treated Steel Components
Failure Analysis of Weldments
Weld Integrity and Performance
High-Carbon Steels—Fully Pearlitic Microstructures and Wire and Rail Applications
Steels: Processing, Structure, and Performance (Second Edition)
Non-Martensitic Strengthening of Medium-Carbon Steels—Microalloying and Bainitic Strengthening
Steels: Processing, Structure, and Performance (Second Edition)
Indentation Hardness Testing of Ceramics
Mechanical Testing and Evaluation
Principles of Shearing, Blanking, and Piercing
Metalworking: Sheet Forming
Equilibrium Phases and Constituents in the Fe-C System
Metallography of Steels Interpretation of Structure and the Effects of Processing