Chapter 6: Bainite
-
Published:2015
Bainite is an intermediate temperature transformation product of austenite. This chapter describes the conditions under which bainite is likely to form. It discusses the effects of alloying on bainitic transformation, the difference between upper and lower bainite, and the influence of solute drag on bainite formation mechanisms. It also discusses the development of ferrite-carbide bainites and their effect on toughness, hardness, and ductility.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Bainite, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 99–112, https://doi.org/10.31399/asm.tb.spsp2.t54410099
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Microstructures, Processing, and Properties of Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Introduction to Steel Heat Treatment
Steel Heat Treating Fundamentals and Processes
Fundamentals of Steel Heat Treatment
Practical Heat Treating Basic Principles
Effects of Composition, Processing, and Structure on Properties of Irons and Steels
Materials Selection and Design
Bainitic Structures
Metallography and Microstructures
Mechanical Behavior of Nonmetallic Materials
Mechanics and Mechanisms of Fracture An Introduction
Non-Martensitic Strengthening of Medium-Carbon Steels—Microalloying and Bainitic Strengthening
Steels: Processing, Structure, and Performance (Second Edition)
Ferritic Stainless Steels
Stainless Steels for Design Engineers
Corrosion of Cast Irons
Corrosion: Materials
Normalizing, Annealing, and Spheroidizing Treatments; Ferrite/Pearlite and Spherical Carbides
Steels: Processing, Structure, and Performance (Second Edition)