Steels: Processing, Structure, and Performance (Second Edition)
Chapter 5: Martensite
-
Published:2015
The formation of martensite is characterized by its athermal transformation kinetics, crystallographic features, and development of fine structure. This chapter describes the diffusionless, shear-type transformation of austenite to martensite and how it affects the morphology and microstructure of heat-treatable carbon steels. It also provides information on lath and plate martensite and how they differ in structure and deformation properties.