206.0, A206.0, and B206.0[1]: Al-Cu High-Strength Premium Casting Alloys
-
Published:2019
Abstract
The 206.0, A206.0, and B206.0 alloys (aluminum alloys 2xxx) are structural castings in the heat-treated temper for automotive and aerospace applications where high tensile and yield strengths with moderate elongations are needed. This datasheet provides information on key alloy metallurgy and fabrication characteristics of these 2xxx series alloys, as well as the effects of processing on their typical physical and mechanical properties.
206.0, A206.0, and B206.0: Al-Cu High-Strength Premium Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 516–519, https://doi.org/10.31399/asm.hb.v02b.a0006555