7175 and 7475: High-Purity Versions of 7075
-
Published:2019
Abstract
Alloys 7175 and 7475 are high-purity versions of 7075 to improve ductility in the transverse direction of thick products. This datasheet provides information on key alloy metallurgy and processing effects on physical and mechanical properties of these 7xxx series alloys. It also provides a fatigue life comparison of these alloys.
You do not currently have access to this chapter.
Citation
7175 and 7475: High-Purity Versions of 7075, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 448–452, https://doi.org/10.31399/asm.hb.v02b.a0006743
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
7475 Controlled-Toughness Sheet and Plate Alloy
Properties and Selection of Aluminum Alloys
Fatigue Spectrum Editing
Mechanics and Mechanisms of Fracture An Introduction
Multiaxial Fatigue
Fatigue and Durability of Structural Materials
Estimating Fatigue Life
Fatigue and Fracture
Parameters for Estimating Fatigue Life
Fatigue and Fracture
Metallic Joints: Mechanically Fastened and Welded
Fatigue and Fracture Understanding the Basics
Nonarbitrary Crack Size Concept for Fatigue Crack Initiation
Mechanics and Mechanisms of Fracture An Introduction
Mean Stress
Fatigue and Durability of Structural Materials
Life Extension and Damage Tolerance of Aircraft
Fatigue and Fracture
Engineering Aspects of Failure and Failure Analysis
Metals Handbook Desk Edition (2nd Edition)