7150: High-Strength Plate and Extrusion Alloy
-
Published:2019
Abstract
This datasheet provides information on composition limits for aluminum alloys 7150 and 7050, and processing effects on mechanical properties of alloy 7150-T7751 plate and 7150-T77511 extrusions.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
7150: High-Strength Plate and Extrusion Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 446–447, https://doi.org/10.31399/asm.hb.v02b.a0006742
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
7055 High-Strength Plate and Extrusion Alloy
Properties and Selection of Aluminum Alloys
Principles of Alloying
Alloying Understanding the Basics
6042 Extrusion Alloy
Properties and Selection of Aluminum Alloys
3105 Sheet Alloy
Properties and Selection of Aluminum Alloys
5754 Al-3.1Mg Alloy
Properties and Selection of Aluminum Alloys
6351 Extrusion Alloy
Properties and Selection of Aluminum Alloys
Precipitation-Hardening Stainless Steels
Stainless Steels for Design Engineers
Mechanical Properties
Understanding How Components Fail (Third Edition)
Vacuum Infusion
Composites
Out-of-Plane Analysis
Composites