Abstract
This datasheet provides information on composition limits for aluminum alloys 7150 and 7050, and processing effects on mechanical properties of alloy 7150-T7751 plate and 7150-T77511 extrusions.
You do not currently have access to this chapter.
Citation
7150: High-Strength Plate and Extrusion Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 446–447, https://doi.org/10.31399/asm.hb.v02b.a0006742
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
7055 High-Strength Plate and Extrusion Alloy
Properties and Selection of Aluminum Alloys
Principles of Alloying
Alloying Understanding the Basics
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Precipitation-Hardening Stainless Steels
Stainless Steels for Design Engineers
Vacuum Infusion
Composites
Out-of-Plane Analysis
Composites
5754 Al-3.1Mg Alloy
Properties and Selection of Aluminum Alloys
6351 Extrusion Alloy
Properties and Selection of Aluminum Alloys
Component Mechanical Properties
Binder and Polymer Assisted Powder Processing
Modeling of Porosity Formation during Solidification
Metals Process Simulation