356.0 and A356.0[1]: Al-Si-Mg High-Strength Casting Alloys
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and applications characteristics of Al-Si-Mg high-strength casting alloys 356.0 and A356.0. Figures illustrate the variation of Charpy impact energy in A356-T6 castings as a function of solution time; and room-temperature aging characteristics for aluminum alloy 356.0-T4. Growth and hardness curves for aluminum alloy 356.0-T4 are also presented.
356.0 and A356.0: Al-Si-Mg High-Strength Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 548–552, https://doi.org/10.31399/asm.hb.v02b.a0006568
Download citation file: